- AutorIn
- Mohd Saif Shaikh Helmholtz-Zentrum Dresden-Rossendorf
- Titel
- Room-temperature telecommunication-wavelength photodetection in silicon via sub-bandgap absorption engineering for photonic integrated circuits
- Zitierfähige Url:
- https://nbn-resolving.org/urn:nbn:de:bsz:14-qucosa2-1020133
- Erstveröffentlichung
- 2026
- Datum der Einreichung
- 28.08.2025
- Datum der Verteidigung
- 16.12.2025
- Abstract (EN)
- This thesis investigates the development of all-silicon photodetectors (PDs) for telecom O- and C-band wavelengths (1300 nm – 1550 nm), addressing a significant challenge in silicon (Si) photonics: the absence of efficient, room-temperature detectors compatible with CMOS large-scale fabrication. While silicon’s intrinsic properties have facilitated advancements in passive photonic functionalities, its weak absorption beyond its bandgap (1.12 eV) has traditionally required the heterogeneous integration of materials like germanium (Ge) or III-V semiconductors, which increases complexity, fabrication cost, and yield, as well as device reliability. Tellurium-doped silicon (Si:Te) emerges as a promising solution, utilizing deep-level impurities to enable sub-bandgap absorption within silicon’s electronic structure. The research presents three key innovations: 1. Lateral PIN chalcogen-doped photodiodes: A planar architecture is introduced, providing compatibility with silicon photonic platforms and enhancing carrier collection through an interdigitated structure. Devices with doping concentrations beyond the solid solubility limit (~1020 cm⁻³, 0.5–1.5 at.% Te) in Si are fabricated via ion implantation and pulsed laser annealing (PLA), achieving room-temperature responsivities of 3×10-2 A/W at 1300 nm and 1×10-2 A/W at 1550 nm. A noise equivalent power (NEP) of ~10-6 W/√Hz at 1550 nm and a 3dB cut-off frequency of 268 kHz is observed for these devices. These values significantly surpass previous work on Si:Te photodetectors, demonstrating an improvement of over 30 times. 2. Carrier dynamics optimization by doping near-solubility: By controlling dopant concentrations near the solid solubility limit (~1016 cm⁻³, 0.0001 at. % Te) and employing meander-shaped active regions, the recombination losses are minimized, and photogenerated carrier collection efficiency is improved. Material characterization quantifies the optimal balance between doping concentration, absorptance, mobility, and carrier lifetime. The strategic optimizations for material property improvements and device design resulted in a significant enhancement of detector performance, achieving a record-high responsivity of 0.05 A/W with an NEP of 3.0x10⁻⁸ W/√Hz. 3. Waveguide integration of Si:Te material: To our knowledge, the first waveguide-integrated Si-doped with Te photodetector has been demonstrated, enabling on-chip light detection. Operating within the optical C band, our detector achieves a responsivity of 0.56 A/W, a quantum efficiency of 44.8%, an NEP of 4.2×10-10 W/√Hz, a linear dynamic range of 33.7 dB, and a bandwidth of 2 GHz, meeting key performance criteria for optical communication systems. This thesis presents a novel framework for photodetection in silicon photonic integrated circuits, eliminating the need for heterogeneous integration with materials such as germanium. The alignment of our approach with conventional silicon processing enhances scalability, cost-effectiveness, and seamless integration with CMOS. Additionally, this platform is poised to propel advancements in mid-infrared sensing and on-chip optical interconnects, where CMOS-compatible detection is crucial.
- Verweis
- Link: https://doi.org/10.48550/arXiv.2412.05872
A high-performance all-silicon photodetector enabling telecom-wavelength detection at room temperature
DOI: 10.48550/arXiv.2412.05872 - Room-temperature telecom Si:Te PIN planar photodiodes: A study on optimizing device dimensions
Link: https://doi.org/10.1016/j.mssp.2024.108515
DOI: 10.1016/j.mssp.2024.108515 - On-chip lateral Si:Te PIN photodiodes for room-temperature detection in the telecom optical wavelength bands
Link: https://doi.org/10.1364/OE.494463
DOI: doi.org/10.1364/OE.494463 - Phase evolution of Te-hyperdoped Si upon furnace annealing
DOI: 10.1016/j.apsusc.2021.150755
Link: https://doi.org/10.1016/j.apsusc.2021.150755 - Temperature-Dependent Dynamics of Charge Carriers in Tellurium Hyperdoped Silicon
DOI: 10.1002/aelm.202400417
Link: https://doi.org/10.48550/arXiv.2412.05872 - International Patent Application No. PCT/EP2025/062564, HZDR Reference-P2408WO, 8th May 2025
- Freie Schlagwörter (DE)
- Tellur-dotiertes Silizium, Chalkogen, Hyperdotierung, Feststofflöslichkeitsdotierung, Ionenimplantation, Infrarot-Fotodetektoren, wellenleiterintegrierte Fotodioden, photonische integrierte Schaltungen, Telekommunikation
- Freie Schlagwörter (EN)
- tellurium doped silicon, chalcogen, hyperdoping, solid-solubility doping, ion-implantation, Infrared-photodetectors, waveguide-integrated photodiodes, photonic integrated circuits, telecom
- Klassifikation (DDC)
- 621
- Klassifikation (RVK)
- ZN 4100
- GutachterIn
- Hon.-Prof. Dr. Artur Erbe
- Prof. Dr. Carsten Ronning
- Den akademischen Grad verleihende / prüfende Institution
- Technische Universität Dresden, Dresden
- Sonstige beteiligte Institution
- Helmholtz-Zentrum Dresden-Rossendorf, Institute of Ion Beam Physics and Materials Research, Dresden
- Version / Begutachtungsstatus
- publizierte Version / Verlagsversion
- URN Qucosa
- urn:nbn:de:bsz:14-qucosa2-1020133
- Veröffentlichungsdatum Qucosa
- 17.02.2026
- Dokumenttyp
- Dissertation
- Sprache des Dokumentes
- Englisch
- Lizenz / Rechtehinweis
- Inhaltsverzeichnis
Table of Contents Declaration of authorship I Abstract III Zusammenfassung IV List of figures V List of tables XI Abbreviations & Acronmys XII Symbols XIV 1 Introduction 1 1.1 Research background and motivation 1 1.2 State-of-the-art devices: all-silicon photodetectors for telecom wavelengths 2 1.3 The challenge of photodetection in silicon 6 1.4 The promise of tellurium-doped silicon 7 1.5 Research Objectives 7 1.6 Thesis Outline 8 2 Semiconductor physics and photodetector key performance metrics 10 2.1 Deep-level impurities in Si and hyperdoping 10 2.2 Optical absorption in semiconductors 14 2.3 Process of photon detection and effect of hyperdoping 17 2.4 Recombination processes 20 2.4.1 Shockley–Read–Hall (SRH) recombination 21 2.4.2 Auger recombination 22 2.4.3 Surface recombination 23 2.5 Carrier transport mechanisms 24 2.6 Types of infrared detectors and their performance metrics 26 2.6.1 Responsivity of a photodetector 27 2.6.2 Noise in photodetectors 27 2.6.3 Individual noise sources 28 2.6.4 Noise Equivalent Power and Detectivity 30 2.6.5 Frequency response 31 2.6.6 Linear dynamic range 32 2.7 Conclusion 33 3 Materials & Methods 35 3.1 Device fabrication methods 35 3.1.1 UV-photolithography 35 3.1.2 Ion-implantation 36 3.1.3 Annealing Techniques 36 3.1.4 Ohmic contact formation 38 3.2 Material characterization 40 3.2.1 Raman Spectroscopy 40 3.2.2 Kelvin probe force microscopy (KPFM) 41 3.2.3 Hall effect measurements 42 3.3 Electro-optical photodetector characterization 42 3.3.1 Experimental setup 42 3.3.2 Spectral response 43 3.3.3 Device characteristics: dark current-voltage (IV) 44 3.3.4 Noise equivalent power (NEP) measurement and benchmarking 44 3.3.5 Frequency response or bandwidth measurement 46 4 On-chip lateral Si:Te PIN photodiodes for room-temperature detection in the telecom optical wavelength bands and their geometric optimization 47 4.1 Introduction 47 4.2 Experimental details 49 4.3 Results and discussion 49 4.3.1 Material synthesis and analysis 49 4.3.2 Dark current-voltage (IV) and telecom-wavelength photoresponse 52 4.3.3 Noise Equivalent Power, Detectivity, and Frequency Response 54 4.4 Discussion on physical mechanisms governing Si:Te PIN photodiode operation 56 4.5 Optimizing device dimensions of the Si:Te PIN (1.5 at. %) detectors 58 4.6 Control device fabrication 63 4.7 Conclusion 64 5 Optimizing carrier dynamics in Si:Te Photodetectors 66 5.1 Introduction 66 5.2 Results and Discussions 66 5.2.1 Devices with Te concentrations exceeding solid solubility limits 67 5.2.2 Interplay between carrier generation and carrier collection based on doping concentration 69 5.2.3 Final Device Implementation with Optimized Strategies 85 5.3 Working principle of the Si:Te meander photodetector 89 5.4 Conclusion 90 6 An all-silicon waveguide-coupled photodetector for room-temperature telecom wavelengths detection 91 6.1 Introduction 91 6.2 Waveguide integrated photodetector (WG-PD) structure 92 6.3 Device fabrication 95 6.4 Device characterization results 100 6.4.1 Calibration of the input optical power 100 6.4.2 Electro-optical characterization 101 6.5 Discussion 108 6.6 Conclusion 108 7 Conclusion and future work 110 7.1 Summary of research 110 7.2 Future works 111 Bibliography 114 Acknowledgement 123 Curriculum vitae 124 Scientific contributions 125